- Chemical Composition: Carbon 0.59 - 0.76%; Manganese 0.30 - 0.80%; Silicon 0.15 - 0.35%; Sulphur 0.030% MAX; Phosphorus 0.030% MAX;
- Tensile Strength: 240,000 to 270,000 psi
- Rockwell Hardness C40 - 48
- Width 0.125 in. +/- 0.005 in.
- Thickness 0.025 in./0.026 in./0.027 in. +/- 0.001 in.
- Length 26 in. +/- 0.125 in.